Dalilai da taka tsantsan don karyewar zanen gadon polycarbonate yayin jigilar kaya
Don adana farashin jigilar kaya, masu amfani sun zaɓi yin mirgine zanen gado na polycarbonate don sufuri. Lokaci-lokaci, zanen gado yana karye. Dalilan haka su ne:
1. National misali polycarbonate zanen gado karya, yayin da wadanda ba misali polycarbonate zanen gado ba. Wannan shi ne saboda ma'auni na polycarbonate na ƙasa suna da nauyin gram mafi girma kuma sun fi wuya fiye da zanen gado mara kyau, yana haifar da mafi girma bayan an yi birgima. Bugu da ƙari kuma, PC polycarbonate yana da mahimmanci ga notches, don haka gefuna na zanen gadon polycarbonate na iya "rasa" idan duwatsu masu kaifi sun taso.
2. An adana rolls ɗin na dogon lokaci. Diamita na zanen gadon polycarbonate da aka yi birgima yana da ƙanƙanta, yana da nisa fiye da yadda aka yarda (yawanci, radius na lanƙwasawa nabiyu-Layer polycarbonate zanen gadoya zama ≥ 175 sau kauri). Lokacin daga naɗaɗɗen lissafin zuwa wurin da aka nufa bai kamata ya wuce sa'o'i uku ba. Bayan isowa, ya kamata a kwance zanen gadon nan da nan kuma a adana su a cikin ɗakin ajiya.
3. Gefuna na zanen gadon polycarbonate an lalata su yayin sufuri. Ana ɗora zanen gadon polycarbonate ɗin da aka yi birgima a kan motar bayan an yi birgima, yana haifar da karce a saman, kuma cunkoson sufuri na iya haifar da tsagewa.


EN
ES
PT
AR
DE
TR
FR
RU
IT